3D Printed Part

Objective Improve Surface Finish & Color (Dye)
Part Description Prototypes
3D Printer Technology 2D Plastic SLS
Material EOS PA 1100
Process Type  Surface Finish & Dying

If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.