Once this prototype thermoform mold is printed, it needs many hours of hand labor to sand down the surface and then polish it to allow the mold to produce a smooth part and to release the part easily after molding.

Objective Improve Surface Finish of Mold
Part Description Prototype Mold
3D Printer Technology HP MJF
Material PA Nylon Powder
Process Type  Multiple Processes 

If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.