PA-1200 3d printed plastic tags

Objective Improve Surface Finish & Dye
Part Description Tags
3D Printer Technology
Material PA – 1200
Process Type  Dying Additive Manufactured Parts

If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.