The customer desired to establish a means of removing powder build material from the MJF technique, without making a powdery mess and keeping the surface color intact.

Objective Remove Build Without a Powdery Mess
Part Description Sample
3D Printer Technology HP Color 580 Plastic MJF
Material HP PA 15 Color
Process Type Water Jet

If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.