3D Printed Electronic Housings, Post-processed
Objective Improve the Surface Finish
Part Description Electronic Housings
3D Printer Technology 3D Plastic MJF
Material HP PA 12
Process Type

If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.