The SLS part was taken from raw printed to consumer quality with color coating, label application, and clear coating.

Finished and coated black pa12 chair model that was 3D printed

Objective Smooth Surface and Coat
Part Description Chair Desk Ornament
3D Printer Technology SLS
Material PA12
Process Type  Multiple Processes plus Coating

If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.