3D printed and post-processed tooth

 

ObjectiveImprove Surface Finish & Polish
Part DescriptionTooth
3D Printer Technology3D Plastic SLA
MaterialVero Clear
Process Type Centrifugal Disc Finisher 

If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.