ObjectiveImprove Surface Finish
Part DescriptionConsumer Pill Box
3D Printer TechnologyMJF
MaterialHP PA 12
Process TypeTumbling Equipment

If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.