Develop alternate designs of the print build for improved post processing

After our meeting, we  suggested  the following design idea as a way to help facilitate the post processing.

Objective Clean & Improve the Surface Finish
Part Description Medical Components: COVID Swabs
3D Printer Technology HP – MJF
Material PA 12
Process Type  

If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.