3D printed automotive mold and post-processed
Objective Sanding 3D Printed Object
Part Description Automotive Mold
3D Printer Technology
Material Wax
Process Type  Vibratory Tumblers

If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.