Objective | Remove Build Material |
Part Description | Automotive Intake Manifold |
3D Printer Technology | 3D Plastic SLS |
Material | Nylon GF (Glass-Filled) |
Process Type | Custom Tumbler |
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.