To evaluate methods for surface processing additive manufactured impellers
Objective | Evaluate process options |
Part Description | Turbine Impeller |
3D Printer Technology | DMLS |
Material | AlSi 10Mg |
Equipment Type | Water Jet |
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.