ObjectivePost-Process Surface Improvement
Part DescriptionPromotional Bottle Opener
3D Printer TechnologyMetal – DMLS
MaterialPost-Processing 3D Metal 17-4
Equipment TypeHigh-Energy Centrifugal Disc Finisher