Objective | Reduce hand polishing |
Part Description | Golf Putter Head |
3D Printer Technology | ExOne Binder Jet |
Material | Bronze- Stainless |
Equipment Type | Water Jet |
If you are unsure what equipment and media you require to achieve your desired surface finish, then send us your part, and we will evaluate it and provide you with a metrology report.